MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Multibase Multi-Pro® 2010 X Natural 20% Filler Content Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Data provided by Multibase.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792-91
Linear Mold Shrinkage 0.0067 cm/cmASTM D955-89
Melt Flow 10 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 46.9 MPaASTM D638-95
Elongation at Break 21 %ASTM D638-95
Flexural Strength 65.9 MPaASTM D790-95
Flexural Modulus 0.250 GPaASTM D790-95
Izod Impact, Notched 0.430 J/cmASTM D256-93a
Gardner Impact 1.70 JASTM D5420-93
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °CASTM D648-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE
A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE
A. Schulman POLYBATCH™ AO-25 Antioxidant Masterbatch Based in LDPE
Multibase Multi-Pro® 2005 XRC Black 20% Filler Content Polypropylene
Braskem F1000HC Homopolymer Polypropylene

PLA245 / 49642

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.