MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sumitomo Bakelite Varcum 29202 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 29202 is an unmodified, one-step, powdered phenolic resin.

APPLICATION:

  • Passenger car brake linings.
  • Passenger car clutch discs.

FEATURES:

  • Provides a very slight softening action under elevated temperature conditions.
  • Contributes to retention of frictional properties under varying temperatures.
  • Exhibits smooth, soft braking action and good pedal feel.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 200 Mesh200 MeshScreen %: < 1.0; DCT 4007A
 
Thermal PropertiesMetricEnglishComments
Softening Point 62.5 °C145 °FCap. Shrink; DCT 4000B
 
Processing PropertiesMetricEnglishComments
Cure Time 0.833 min
@Temperature 150 °C
0.0139 hour
@Temperature 302 °F
DCT 4001A
 
Descriptive Properties
Inclined Plate Flow62.5[mm]; DCT 4009A; hot; at 125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUMIT687 / 194492

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.