MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

Saint-Gobain Meldin® 5210 Polyketone
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: This grade provides a very low coefficient of friction, especially against steel surfaces. It is used specifically for steering system yokes.

Having a high tensile, compressive and flexural strength, Meldin® 5000 materials are injection molded into tight-tolerance finished components in simple or complex designs that can exhibit metal-like finishes without expensive machining or secondary operations, and with the advantages of being lighter and corrosion resistant.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ASTM D792
Water Absorption 0.17 %
@Temperature 23.0 °C,
Time 86400 sec
0.17 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  10.0 MPa
@Temperature 249 °C
1450 psi
@Temperature 480 °F
ASTM D638
 70.0 MPa
@Temperature 23.0 °C
10200 psi
@Temperature 73.4 °F
ASTM D638
Elongation at Break 6.6 %6.6 %ASTM D638
Tensile Modulus 3.20 GPa464 ksiASTM D638
Flexural Strength  8.00 MPa
@Temperature 249 °C
1160 psi
@Temperature 480 °F
ASTM D790
 123 MPa
@Temperature 23.0 °C
17800 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus 3.20 GPa464 ksiASTM D790
Compressive Strength  16.0 MPa
@Temperature 200 °C
2320 psi
@Temperature 392 °F
ASTM D695
 108 MPa
@Temperature 23.0 °C
15700 psi
@Temperature 73.4 °F
ASTM D695
Compressive Modulus 2.90 GPa421 ksiASTM D695
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FASTM D3418
Glass Transition Temp, Tg 143 °C289 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ112b / 305350

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.