Two-side coated, one-side sealable OPP film designed for use in high speed or demanding, horizontal packaging applications. The low temperature seal coating delivers a low seal initiation temperature and wide operating range. LMBs PVdC surface is an excellent surface for printing and provides an advanced level of moisture barrier. Information provided by ExxonMobil Chemical |