MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arla ATECH® 5100 (70/30) PC/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ATECH® 5100 (70/30) is PC/ABS sheet coextruded with matte ABS layer. The product offers good impact strength and wide working temperature range. ATECH® 5100 has good chemical resistance to most common chemicals and offers better fire performance than ABS.

Also Available: ATECH 5103 with extra UV stabilizers added to improve weather resistance; ATECH 5110 with the matte surface on both sides
Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met.

Benefits: matte surface finish after thermoforming; Easy to thermoform; High impact strength; Good thermal qualities

Application: Suitable for demanding automotive parts which are exposed to secondary UV light, and other tough industrial applications where a supermatt finish is required.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 87.0 MPaISO 2039
Tensile Strength at Break 40.0 MPaISO 527
Tensile Strength 45.0 MPaISO 527
Tensile Strength, Yield 45.0 MPaISO 527
Elongation at Break >= 4.0 %at Tensile strength; ISO 527
 50 %ISO 527
Elongation at Yield >= 4.0 %ISO 527
Modulus of Elasticity 2.05 GPaISO 527
Flexural Strength 73.0 MPaISO 178
Flexural Modulus 2100 MPaISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 25.0 kJ/m²
@Temperature -23.0 °C
ISO 180/1A
 38.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact, Notched 23.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1/1eA
 25.0 kJ/m²
@Temperature -23.0 °C
ISO 179-1/1eA
 37.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75
Vicat Softening Point 125 °CB120; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
Flame Spread <= 5.00 mm/min
@Thickness 3.00 mm
US-FMVSS 302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARLA913 / 301091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.