MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds EpoxAmite® HT; Hardener: HT High Temp Laminating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: EpoxAmite® HT High Temperature Laminating Epoxy is a water clear, UV resistant laminating epoxy that resists high temperatures up to 300°F / 149°C when properly cured. Pot life is 1 hour and cure time is 24 hours at 73°F / 23°C (post cure required – see post cure schedule). Ultra-low viscosity ensures uniform wetting out and fast penetration of reinforcement materials during hand lay-up or vacuum infusion processes. Cured resin offers superior physical properties. EpoxAmite® HT High Temp Laminating Epoxy can be used with S-Glass, E-Glass, Kevlar and carbon fibers for making composite tooling or parts. Applications include making high temperature pre-preg parts, bonding fixtures, vacuum form molds and prototype injection molds. Use as a backup laminating resin for EpoxAcoat® HT high temperature surface coat epoxy.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D-1475
Viscosity 650 cP650 cPMixed; ASTM D-2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D-2240
Tensile Strength, Ultimate 44.8 MPa6500 psiafter 7 days at 73°F/23°C.; ASTM D-638
 221 MPa32100 psitesting conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C; ASTM D-638
Elongation at Break 2.3 %2.3 %ASTM D-638
Tensile Modulus 2.36 GPa342 ksiafter 7 days at 73°F/23°C.; ASTM D-638
 14.8 GPa2150 ksitesting conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C; ASTM D-638
Flexural Strength 84.978 MPa12325 psiafter 7 days at 73°F/23°C.; ASTM D-790
 143 MPa20700 psitesting conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C; ASTM D-790
Flexural Modulus 2.96 GPa429 ksiafter 7 days at 73°F/23°C.; ASTM D-790
 15.28 GPa2216 ksitesting conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C; ASTM D-790
Compressive Strength 114 MPa16600 psiASTM D-695
Compressive Modulus 1.16 GPa168 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °FHeat Deflection Temperature; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourThin Film Working Time
 1440 min24.0 hour
Pot Life 60.0 min60.0 minASTM D-2471
 
Descriptive Properties
ColorClear
Mix Ratio100A:33Bby weight
Specific Volume25.2[in3/lb], ASTM D-792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN189 / 296890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.