MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ CATA 3040 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL™ RTV 3040 is a clear, high strength, addition cure silicone rubber compound. It is formulated to be used with multiple catalysts to cure overnight at room temperature or within hours at elevated temperature to give a variety of hardness. Its low viscosity makes the product easy to pour and quick to degas. BLUESIL™ RTV 3040 is designed to serve the needs of the prototype by reproducing intricate details and maintaining tight tolerances. In addition, BLUESIL™ RTV 3040 has been formulated to provide improved urethane resin resistance. BLUESIL™ RTV 3040 system is compliant to 21CFR177.2600 ~ Repeated food contact applications.

Applications:

  • Conventional production and prototype molds
  • Finished rubber parts
  • Stereolithography (SLA) molds

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
Viscosity 40000 cPMixed
 50000 cPPart A, Base Component
Linear Mold Shrinkage <= 0.0010 cm/cm
@Time 86400 sec
 <= 0.0010 cm/cm
@Time 605000 sec
Storage Temperature 24.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38ASTM D2240
Tensile Strength 920 psiASTM D412
Elongation at Break 340 %ASTM D412
Tear Strength 120 pliASTM D624, Die B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 4.00 hour
@Temperature 40.0 - 65.0 °C
accelerated, heat curing may increase shrinkage
 24.0 hour
@Temperature 24.0 °C
50% RH
Pot Life 120 min
Working Life 1.00 hour
Shelf Life 18.0 Month
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorTranslucentPart A, Base Component
 TranslucentPart B, Catalyst Component
Mix Ratio10:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ CATA 3020 HT Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ CATA 3038 Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ CATA 3045 Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ V-340 CA-55 Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ V-330 CA-35 Silicone Rubber

PBLUST032 / 191008

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.