MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Sahara Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic

Material Notes: Sahara Films are developed for use in applications where increased temperature resistance is desired.

Applications/Uses

  • High temperature printable films
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.22 g/ccASTM D792
    Water Vapor Transmission 8.00 g/m²/dayASTM F372
    Oxygen Transmission 18.0 cc-mm/m²-24hr-atmASTM D3985
    Carbon Dioxide Transmission 87.0 cc-mm/m²-24hr-atmASTM D1434
    Thickness 250 micronsASTM D374
     
    Mechanical PropertiesOriginal ValueComments
    Film Tensile Strength at Yield, MD 54.0 MPaASTM D882
    Film Tensile Strength at Yield, TD 52.0 MPaASTM D882
    Film Elongation at Break, MD 150 %ASTM D882
    Film Elongation at Break, TD 130 %ASTM D882
    Film Elongation at Yield, MD 6.0 %ASTM D882
    Film Elongation at Yield, TD 6.0 %ASTM D882
    Tensile Modulus 1.90 GPaTangent, MD; ASTM D882
    Tear Strength, Total 3.90 NSplit Tear Method, 254mm/min, MD; ASTM D1938
     4.10 NSplit Tear Method, 254mm/min, TD; ASTM D1938
     42.0 N90° Tear Resistance, MD; ASTM D1004
     43.0 N90° Tear Resistance, TD; ASTM D1004
    Elmendorf Tear Strength, MD 2.68 g/micronASTM D1922
    Elmendorf Tear Strength, TD 3.68 g/micronASTM D1922
    Dart Drop 2.38 g/micronASTM D1709A
    Film Tensile Strength at Break, MD 49.0 MPaASTM D882
    Film Tensile Strength at Break, TD 44.0 MPaASTM D882
    1% Secant Modulus, MD 1800 MPaASTM D882
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 1.00e+17 ohm-cmASTM D257
    Surface Resistivity per Square 1.00e+16 ohmASTM D257
    Dielectric Constant 2.34
    @Frequency 1e+6 Hz
    ASTM D150
     2.46
    @Frequency 1000 Hz
    ASTM D150
    Dielectric Strength 50.0 kV/mmShort Time, 500V/sec; ASTM D149
    Dissipation Factor 0.0050
    @Frequency 1000 Hz
    ASTM D150
     0.014
    @Frequency 1e+6 Hz
    ASTM D150
     
    Thermal PropertiesOriginal ValueComments
    Glass Transition Temp, Tg 100 °CDSC
     
    Optical PropertiesOriginal ValueComments
    Refractive Index 1.566
    @Wavelength 589.3 nm
    nD; ASTM D542
    Haze <= 1.0 %ASTM D1003
    Gloss 106 %at 60°; ASTM D2457
    Yellow Index 0.63 %ASTM D2244
    Transmission, Visible 90 %Regular Transmittance; ASTM D1003
     92 %Total Transmittance; ASTM D1003
     100 %Transparency; ASTM D1746
     
    Descriptive Properties
    Color, CIE a*-0.02VGAS-A-AN-G-RS-001
    Color, CIE b*0.34VGAS-A-AN-G-RS-001
    Color, CIE L*96.14VGAS-A-AN-G-RS-001
    Whiteness Index, ASTM D224488.82

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    PE9097 / 35153

    Rulon Bearings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.