KYDEX® FST03 is a proprietary, high performance thermoplastic sheet formulated to meet all Boeing and Airbus toxicity requirements for aircraft interior components. Its integral pearlescence adds a new dimension to aviation interior design. KYDEX® FST meets all flame, smoke, and heat release requirements set forth in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) as well as toxicity requirements for Airbus (ABD003) and Boeing (BSS7239). Its excellent thermoforming characteristics make it an ideal material for three-dimensional components where pearlescent design effects are desirable. Suggested Application: - Seat parts
- Bulkhead laminates
- Life vest shrouds
- Passenger service units
- Monitor Shrouds
- Armrests
- Molding strips
- Tray tables
- Kick panels
Features: - Integral pearlescent effect
- Meets the stringent requirements of FAR 25.853 (a) and (d) in all thicknesses and colors
- Meets toxicity smoke requirements of Airbus (ABD0031) and Boeing (BSS7239)
- Excellent fabrication and formability characteristics
- Allows for tight tolerance control
- Available in a wide range of integral colors
Information provided by SEKISUI KYDEX, LLC. |