MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Potters Industries Coarse Grade Oil Drilling Beads
Categories: Ceramic; Glass

Material Notes: Potters Industries’ Oil Drilling Coarse Grade glass beads are designed for oil drilling mud applications to reduce friction and torque within deviated holes. Potters solid glass spheres act as tiny ball bearings to reduce friction and reduce differential pressure. The glass beads are a transparent, solid soda Lime glass, free of pits and excess air bubbles. The glass beads are chemically inert and do not affect the chemical characteristics of the mud system.

Information provided by Potters Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/cc
Particle Mesh Size 20 - 40 Mesh
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.0 - 6.0
Compressive Strength >= 30000 psi
 
Descriptive Properties
Round>75%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Potters Industries Fine Grade Oil Drilling Beads
Mateck Sodium Chloride (NaCl)
Guadua Bamboo
Moso Bamboo
Sodium Chloride, NaCl (Halite)

CPOT8048 / 184674

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.