Hostacom ERC 450N NA PG05 Black is a high stiffness, scratch resistant, mineral-filled thermoplastic elastomeric olefin (TEO) resin that is typically used for automotive interior applications. Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: High Stiffness; Scratch Resistant Information provided by LyondellBasell. |