MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nickel Gear Bronze, UNS C91700, Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Property data for as-cast specimens.

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, and Sand.

Applications: Worm gears, steel mill nuts

Classified under: Tin bronze

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 85
Tensile Strength, Ultimate 305 MPa
Tensile Strength, Yield 150 MPa
Elongation at Break 16 %in 50 mm
Modulus of Elasticity 105 GPa
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000017241 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 71.0 W/m-K
@Temperature 20.0 °C
Melting Point 850 - 1015 °C
Solidus 850 °C
Liquidus 1015 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 85 - 87.5 %
Lead, Pb <= 0.25 %
Nickel, Ni 1.3 - 2.0 %
Phosphorus, P <= 0.30 %
Tin, Sn 11.3 - 12.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded Tin Bronze, UNS C92500, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Nickel Gear Bronze, UNS C91700, Centrifugal or Permanent Mold Cast
Nickel Tin Bronze, UNS C94700, Copper Casting Alloy
Tin Bronze, UNS C90700, Sand castings

MC91700b1 / 11936

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.