MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain CHR® 2916-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2915 and 2916 are manufactured from heat-resistant fibreglass cloth backing coated with high-temperature silicone adhesive.

Features/Benefits: CHR® 2915 and 2916 are exceptionally strong abrasion-resistant tapes providing maximum solvent resistance. They have excellent temperature resistance and are thermally stable. They can be used in applications that require continuous temperatures of up to 260 °C and its abrasion resistance makes them extremely durable products. 2915-7 meets MIL-I-19166C U.S. Government specifications.

Applications: CHR® 2915 and 2916 are very versatile tapes. Applications range from general industry electrical maintenance to high-temperature splicing and wrapping. Some specific applications are over-wrap on motor rewinds, protective wrapping for wire and cables and hightemperature masking tape for welding stainless steel. CHR® 2915 and 2916 also perform as light duty plasma or flame spray masking tapes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tear Strength 28.9 kN/m165 pliTensile Strength
Peel Strength 0.490 kN/m2.80 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 4300 V4300 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® SG56-05(R) Anti-Static Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® SG25-05(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® M897 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® K250 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® C680 Paper Backing Silicone Adhesive Pressure Sensitive Tape

PSTGQZ379 / 68893

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.