MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Duracon® ES-5 Acetal Co-polymer (POM), Conductive, Antistatic
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.

The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O) and carbon-carbon (-C-C- bond) comonomer groups are incorporated into its main chain. Therefore the copolymer has superior chemical and thermal stability, compared with acetal homopolymer.

Acetal co-polymer is well-balanced in terms of mechanical, chemical and thermal properties, and its superior moldability allows it to be widely employed in various industrial fields.

Information provided by PolyPlastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 49.0 MPa7110 psiISO 527-1, 2
Elongation at Break 7.5 %7.5 %ISO 527-1, 2
Tensile Modulus 2.70 GPa392 ksiISO 527-1, 2
Flexural Strength 84.0 MPa12200 psiISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 ohm-cm100 ohm-cmIEC 60093
Surface Resistance 500 ohm500 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 109 °C228 °FISO 75-1, 2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duracon® EB-10 Acetal Co-polymer (POM), Conductive, Antistatic
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General
Polyplastics Duracon® M270-48 Acetal Co-polymer (POM), Antistatic, High flow
RTP Company ESD 881 Acetal (POM), Carbon Fiber - Electrically Conductive
RTP Company EMI 863 Acetal (POM); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PPOLPL041 / 57034

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.