MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shanghai Potomer FKM 03A80 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Character: Fluoroelastomer is white/amber and semi-transparent elastomer and it is odorless, nontoxic, non-flammable. Fluoroelastomer owns excellent resistance to heat, oil and chemicals and it has outstanding physical-mechanical properties and resistance to weathering and can be dissolved in low M.W ketones and esters.

Features: Middle and high viscosity, good milling and calendering performance.

Main Applications: Calendaring sheet, skeletal oil seal, extruded hose etc.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 70 - 90
@Temperature 121 °C
70 - 90
@Temperature 250 °F
ML (1+10)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 8.00 MPa1160 psi
 7.00 MPa
@Temperature 275 °C,
Time 86400 sec
1020 psi
@Temperature 527 °F,
Time 24.0 hour
After aging
Elongation at Break 160 %160 %
 150 %
@Temperature 275 °C,
Time 86400 sec
150 %
@Temperature 527 °F,
Time 24.0 hour
After aging
Compression Set 55 %
@Temperature 200 °C,
Time 86400 sec
55 %
@Temperature 392 °F,
Time 24.0 hour
compression rate 30%
 
Descriptive Properties
Solvent Resistance51# aviation kerosene, 200 X 24hr, measured by weight increment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM079 / 284525

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.