MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BST Elastomer BSTE SBR0122 E-SBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Oil Extended Emulsion Styrene Butadiene Rubber

Information provided by Bangkok Synthetics Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %Raw Polymer; ASTM D5668-19
Mooney Viscosity  47 - 57
@Temperature 100 °C
47 - 57
@Temperature 212 °F
ML1+4, Raw Polymer; ASTM D1646-19a
 58 - 70
@Temperature 100 °C
58 - 70
@Temperature 212 °F
ML1+4, Compound; ASTM D1646-19a
Ash <= 1.5 %<= 1.5 %Raw Polymer; ASTM D5667-95
 
Chemical PropertiesMetricEnglishComments
Styrene Content 35.5 - 38.5 %35.5 - 38.5 %Bound, Raw Polymer; ASTM D5775-95
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 19.1 MPa
@Temperature 145 °C,
Time 2100 sec
>= 2770 psi
@Temperature 293 °F,
Time 0.583 hour
Compound; ASTM D412-16
Elongation at Break >= 480 %
@Temperature 145 °C,
Time 2100 sec
>= 480 %
@Temperature 293 °F,
Time 0.583 hour
Compound; ASTM D412-16
300% Modulus  6.30 - 11.1 MPa
@Temperature 145 °C,
Time 1500 sec
914 - 1610 psi
@Temperature 293 °F,
Time 0.4167 hour
Compound; ASTM D412-16
 8.30 - 13.1 MPa
@Temperature 145 °C,
Time 2100 sec
1200 - 1900 psi
@Temperature 293 °F,
Time 0.583 hour
Compound; ASTM D412-16
 9.40 - 14.2 MPa
@Temperature 145 °C,
Time 2990 sec
1360 - 2060 psi
@Temperature 293 °F,
Time 0.830 hour
Compound; ASTM D412-16
 
Descriptive Properties
Content<0.5%Soap, Raw Polymer, ASTM D5774-95
 1Stearic Acid, ASTM D3185 - 06
 1.34Accelerator (TBBS), ASTM D3185 - 06
 1.75Sulfur, ASTM D3185 - 06
 134Raw SBR0122, ASTM D3185 - 06
 23.9-26.9%Oil, Raw Polymer, ASTM D5774-95
 3Zinc Oxide, ASTM D3185 - 06
 4.2-6.2%Organic Acid, Raw Polymer, ASTM D5774-95
 67HAF Black (IRB#7), ASTM D3185 - 06

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBSTEL001 / 315732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.