Asahi Kasei Leona™ TR161 Polyamide 66, Heat Stabilized, Impact
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Heat Stabilized
Material Notes:
Applications: Automotive parts, electrical & electronic parts, parts for office furnishings.
Information provided by Asahi Kasei Corp.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.11
g/cc
1.11
g/cc
Dry as Molded; ASTM D792
Density
1.11
g/cc
0.0401
lb/in³
Dry as Molded; ISO 1183
Moisture Absorption at Equilibrium
1.9 %
@Temperature 23.0 °C
1.9 %
@Temperature 73.4 °F
50% RH; ISO 62
1.9 %
@Temperature 23.0 °C
1.9 %
@Temperature 73.4 °F
50% RH
Linear Mold Shrinkage, Flow
0.017
-
0.022
cm/cm
0.017
-
0.022
in/in
Asahi Kasei
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
98
98
Conditioned at 50% RH; ISO 2039
114
114
Dry as Molded; ISO 2039
Tensile Strength at Break
64.0
MPa
9280
psi
Dry as Molded; ISO 527
Tensile Strength
47.0
MPa
6820
psi
Conditioned at 50% RH; ASTM D638
70.0
MPa
10200
psi
Dry as Molded; ASTM D638
Tensile Strength, Yield
46.0
MPa
6670
psi
Conditioned at 50% RH; ISO 527
72.0
MPa
10400
psi
Dry as Molded; ISO 527
Elongation at Break
15 %
15 %
Dry as Molded; ISO 527
>= 100 %
>= 100 %
Conditioned at 50% RH; ISO 527
Elongation at Yield
4.5 %
@Temperature 23.0 °C
4.5 %
@Temperature 73.4 °F
Dry as Molded; ISO 527
22 %
@Temperature 23.0 °C
22 %
@Temperature 73.4 °F
Conditioned at 50% RH; ISO 527
Tensile Modulus
1.10
GPa
160
ksi
Conditioned at 50% RH; ISO 527
2.40
GPa
348
ksi
Dry as Molded; ISO 527
Flexural Strength
38.0
MPa
5510
psi
Conditioned at 50% RH; ISO 178
88.0
MPa
12800
psi
Dry as Molded; ISO 178
Flexural Modulus
1.00
GPa
145
ksi
Conditioned at 50% RH; ISO 178
2.20
GPa
319
ksi
Dry as Molded; ISO 178
Izod Impact, Notched
1.67
J/cm
3.13
ft-lb/in
Dry as Molded; ASTM D256
12.0
J/cm
22.5
ft-lb/in
Conditioned at 50% RH; ASTM D256
Charpy Impact Unnotched
NB
NB
Conditioned at 50% RH; ISO 179
NB
NB
Dry as Molded; ISO 179
Charpy Impact, Notched
1.50
J/cm²
7.14
ft-lb/in²
Dry as Molded; ISO 179
NB
NB
Conditioned at 50% RH; ISO 179
Taber Abrasion, mg/1000 Cycles
7.0
7.0
Conditioned at 50% RH; ASTM D1044
Thermal Properties
Metric
English
Comments
CTE, linear
70.0
µm/m-°C
38.9
µin/in-°F
Dry as Molded; ASTMD 696
Deflection Temperature at 0.46 MPa (66 psi)
209
°C
408
°F
Dry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
66.0
°C
151
°F
Dry as Molded; ISO 75
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aclo Accucomp Polycarbonate POL051L Medium Viscosity
Aclo Accucomp Polycarbonate POL052L High Viscosity
Asahi Kasei Leona™ TR382 Polyamide 66, Heat Stabilized, Impact
LyondellBasell Hostacom EKC 133N G31325 Polypropylene Copolymer, 16% Talc Filled
LyondellBasell Hifax TRC 2044X BLACK Polypropylene, Talc Filled Elastomer
PASAHI8158 / 221185
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.