MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Domo TECHNYL® A 216 S30 PA66, 30% glass spheres, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Bead Filled

Material Notes: Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.

Available in: Europe

Product Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is recommended for mechanical components which require a very good surface finish with low warpage, and good compression strength. This product is available in natural, black, grey, red, white, and in special colors on request

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psiISO 527 Type 1A
Tensile Modulus 2.50 GPa363 ksiISO 527 Type 1A
Flexural Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 1.90 GPa276 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 5.00e+11 ohm5.00e+11 ohmIEC 60093
Dielectric Strength 26.0 kV/mm660 kV/inIEC 60243
Dissipation Factor 0.110.11IEC 60250
Comparative Tracking Index 500 V500 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY
Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned
Domo TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Dry)
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned)

PRHOD597 / 137828

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.