MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChenGuang CGF-218K PTFE Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Molecular Formula: [CF2--CF2]n

CAS No. 9002-84-0

Description: In addition to all excellent properties of PTFE material, CGF-218 series powders has outstanding performance in paste extrusion to manufacture sealing tape, etc.. The resin are processed by mixing them with some organic solvents to obtain paste which are made into coherent, smooth and flat semifinished products after ram extrusion. During this progression the extruding pressure remains steady .The semifinished products can be further processed to produce unsintered tape by calendering, elongating and removing solvent with heat, and also to manufacture sintered coherent thin-walled tubing , continuous long rod, and wire & cable coating, etc.

Main Applications: Oil-free unsintered broad tape for cutting apart

Extrudate appearance: flat, smooth and coherent

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.19 - 2.25 g/cc2.19 - 2.25 g/cc
Bulk Density 0.320 - 0.520 g/cc0.0116 - 0.0188 lb/in³
Particle Size 600 - 900 µm600 - 900 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.0 MPa3340 psi
Elongation at Break 300 %300 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.040 %<= 0.040 %
 
Descriptive Properties
Heat Instability Index50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU033 / 255632

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.