MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraiburg TPE THERMOLAST® M TM7APO Thermoplastic Elastomer (MC/AD/PA Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The MC/AD/PA series is a material solution for applications requiring basic medical approvals such as ISO 10993-5. The series is characterized by its adhesion to various polyamides, such as PA6 and PA12. The compounds are available in natural colors and can be colored in a variety of ways. They are produced exclusively on a special medical unit.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
Typical applications:
  • Soft touch application (e.g. handles or push buttons)
  • Flexible Connections
  • Membranes
Material advantages:
  • Adhesion to PA6 and PA12
  • Smooth touch
  • Sterilizable (ß-/y-radiation 2x35 kGy, EtO)
  • KRAIBURG TPE Medical Service Package
  • Free from animal ingredients
  • Colorable, also in effect colors

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccDIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70DIN ISO 48-4
Tensile Strength 8.50 MPa200 mm/min; DIN 53504/ISO 37
Elongation at Break 460 %200 mm/min; DIN 53504/ISO 37
Tear Strength 20.0 kN/mISO 34-1 Method B (b)
 
Descriptive Properties
Adhesion to PA126.5 N/mm (B/D)VDI 2019 two-component injection
Adhesion to PA65.0 N/mm (B)VDI 2019 two-component injection
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKRAIA8384 / 309048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.