MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Honeywell TIP 1500 Thermal Insulator Pad
Categories: Other Engineering Material

Material Notes: Benefits And Features:
  • High thermal performance
  • High breakdown voltage
  • Good resistant to tears, cut-throughs and punctures
  • Single side PSA available for easy assembly
Overview: Honeywell TIP1500&TIP3500 thermal insulators are designed to provide low thermal impedance and high isolation for high power and high voltage applications. Integrated fiberglass reinforcement protects the pad from tears, cut-throughs and punctures. TIP1500 and TIP3500 are designed to be soft and conformal which provide excellent mating surface for low pressure mounting. TIP1500 only offers 0.19mm and 0.23mm thickness. TIP3500 offers in thicknesses ranging from 0.25mm to 0.50mm.

Typical Applications:

  • Automotive electronics
  • Power conversion equipment
  • Power supply equipment
  • Motor controllers
  • Speaker amplifier
  • Power switch

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.21 g/cc2.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Dielectric Constant >= 5.5
@Frequency 1e+6 Hz
>= 5.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Breakdown >= 6000 V>= 6000 VASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°FASTM D5470
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorPink
Thickness Range (mm)20.19-0.23ASTM D374

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHONWL6032 / 255362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.