MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell CirculenRecover C14 HP456J Polypropylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: CirculenRenew C14 HP456J is part of the Circulen© product family of circular and sustainable solutions. CirculenRenew C14 polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw materials made from bio-based waste and residue oils. The renewable content of CirculenRenew C14 is measured by an accredited third party laboratory and stated as a parameter on the Certificate of Analysis (CoA). CirculenRenew C14 HP456J is a drop-in solution and therefore doesn’t require any adaptation of the existing processing equipment. CirculenRenew C14 HP456J is a polypropylene homopolymer used for extrusion and thermoforming applications. CirculenRenew C14 HP456J is formulated with a low water-carry-over additive package. Typical applications are monofilaments, ropes, tapes and films.

Status: Commercial - Active

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; South & Central America

Application: Cast Stretch Film; General Purpose Film Packaging; Raffia/Tapes/Strapping; Strapping

Market: Textile

Processing Method: Tapes & Raffia

Attribute: Homopolymer

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 3.40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 21.0 MPa3050 psi50 mm/min; ISO 527-1, -2
Tensile Strength, Yield 34.0 MPa4930 psi50 mm/min; ISO 527-1, -2
Elongation at Break 200 %200 %50 mm/min; ISO 527-1, -2
Elongation at Yield 11.0 %11.0 %50 mm/min; ISO 527-1, -2
Flexural Modulus 1.50 GPa218 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 156 °C313 °FA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9076 / 324011

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.