MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on to a substrate offers excellent permeability to moisture vapor while remaining waterproof and offering an excellent barrier layer to bacteria. This SP grade is specifically designed for outdoor application that needs excellent weather resistance properties.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 1.02 g/ccCond.; ISO 1183
Water Absorption 28 %Dry; Sim. to ISO 62
Moisture Absorption 1.00 %Dry; Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35
@Time 15.0 sec
Dry; ISO 7619-1
Elongation at Break >= 50 %Cond.; ISO 527-1/-2
Tensile Modulus 45.0 MPaCond.; ISO 527-1/-2
50% Modulus 7.00 MPa
@Strain 50 %
Cond.; ISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 158 °C10°C/min; Dry; ISO 11357-1/-3
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveYes
Processing MethodsCalandering
 Casting
 Film Extrusion
 Other Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® MH 1657 Polyether Block Amide (PEBA)
Arkema Pebax® MV 2080 Polyether Block Amide (PEBA)
Arkema Pebax® MH 2030 Polyether Block Amide (PEBA)

PARKG734 / 142529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.