MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT HANSA LPW 721 Microemulsion
Categories: Other Engineering Material

Material Notes: Description: This product can be used in leather top coat to achieve a very peculiar touch. Other properties can be obtained according to the specific application.

Key Features

  • Dry touch
  • Natural appearance in the top coat
  • Imparts a polish effect
  • Very good compatibility with organic compounds
Key Applications
  • Suitable for any kind ot leather
Application: HANSA® LPW 721 is a microemulsion of an organo-modified polysiloxane and a silicon quat. It can be used as a touch modifier to give a dry touch without influencing the natural appearance in the top coat. It increases the surface smoothness and provides a polish effect to the leather. HANSA® LPW 721 shows a good compatibility with organic compounds and can be used in a cationic top coat. HANSA® LPW 721 can be diluted with water to any ratio. The optimal application amount must be adapted to the desired effect. We generally recommend an application amount of 1 – 5%.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 29 - 31 %
pH 5.5 - 6.5
Storage Temperature <= 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Monthif properly stored in closed original containers
 
Descriptive Properties
AppearanceClear liquid (microemulsion)
ChemistryOrgano-modified polysiloxanes and silicone quat
IonicitySlightly cationic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL328 / 314811

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.