LORD Chemlok® 8009 aqueous (water-based) primer is designed to bond elastomers to metals and other substrates when used with Chemlok water-based or solvent-based covercoat adhesives. It is composed of a mixture of dispersed mineral fillers, organic compounds, resins and polymer lattices in an water-based medium.All information provided by Lord. |