MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kraiburg TPE THERMOLAST® K TC7MUZ Thermoplastic Elastomer (UV/AD2 Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The UV/AD2 series is a material solution for applications requiring UV resistance and adhesion to polar thermoplastics such as PC, ABS, PC/ABS, ASA and PMMA. It is particularly suitable for automotive exterior applications. The compounds are available in black.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Black
Typical applications:
  • Window encapsulations
  • Roof rim covers
  • Water deflectors
  • Door sills
  • Trunk openers
  • Front triangles
  • A/B/C/D cappings and covers
  • Rear spoilers
Material advantages:
  • Adhesion to PC, ABS, PC/ABS, ASA, SAN
  • Surface mapping
  • Weather resistant, suitable for automotive exterior
  • Optimized mechanical properties
  • Optimized flow properties
  • Temperature stability up to 90 °C

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³DIN EN ISO 1183-1
Spiral Flow 41.0 cm
@Pressure 76.0 MPa,
Temperature 200 °C
16.1 in
@Pressure 11000 psi,
Temperature 392 °F
DSOP Lab 2032
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575DIN ISO 48-4
Tensile Strength 12.0 MPa1740 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 640 %640 %200 mm/min; DIN 53504/ISO 37
Tear Strength 28.0 kN/m160 pliISO 34-1 Method B (b)
 
Descriptive Properties
Adhesion to ABS8.0 N/mm (C)VDI 2019 two-component injection
Adhesion to ASA9.0 N/mm (C)VDI 2019 two-component injection
Adhesion to PC6.0 N/mm (C)VDI 2019 two-component injection
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8322 / 308986

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.