MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Brasnox DM-50 Methyl ethyl ketone peroxide in dimethyl phthalate
Categories: Other Engineering Material

Material Notes: Brasnox DM-50 is a medium-reactive, general purpose MEKP with low water content.

CAS number: 1338-23-4

EINECS/ELINCS No.: 215-661-2

Applications: Brasnox DM-50 is a general purpose methyl ethyl ketone peroxide (MEKP) for the curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. The curing system Brasnox DM-50/cobalt accelerator is particularly suitable for the curing of gel coat resins, laminating resins, lacquers and castings; moreover the manufacture of light resistant parts may be possible contrary to the curing system benzoyl peroxide/amine accelerator.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.18 g/cc0.0412 - 0.0426 lb/in³
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 3.0 %<= 3.0 %
 
Descriptive Properties
AppearanceClear and colorless liquid
Content8.80-9.00 %Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY436 / 285959

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.