MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cossa Polimeri ESTACARB 0820 GF V0 HF Flame Retardant Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Polycarbonate with 10% glass fiber reinforcement

Flame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good processability, good light resistance

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D 955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psiASTM D 638
Elongation at Break 4.0 %4.0 %ASTM D 638
Flexural Modulus 3.50 GPa508 ksiASTM D 790
Izod Impact, Notched 1.10 J/cm
@Temperature 23.0 °C
2.06 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 135 °C275 °FI.E.C. 335-1
Vicat Softening Point  147 °C
@Load 5.00 kg
297 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
 150 °C
@Load 0.999 kg
302 °F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Glow Wire Test 960 °C1760 °FI.E.C. 695-2-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A380.0-F Die Casting Alloy
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Covestro Makrolon® 9415(Z) Polycarbonate
Covestro Makrolon® 2805 Polycarbonate, Injection Grade
Covestro Makrolon® 2207 Polycarbonate, Injection Grade

PCOSSA911 / 156501

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.