MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave: Polyethylene
Side 2: Uncured Silicone Rubber
Substrate: Style 7628 Fiberglass
Side 1: Cured Silicone Rubber

Appearance: Gray gum on glass fiber fabric

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³Silicone Property, Side 1; Arlon SQA-TMS-024
 1.23 g/cc0.0444 lb/in³Silicone Property, Side 2; Arlon SQA-TMS-024
Thickness 76.2 microns3.00 milInterleave
 102 microns4.00 milSide 1
 203 microns8.00 milSide 2
 203 microns8.00 milSubstrate
 508 microns20.0 milOverall
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4343Silicone Property, Side 2; ASTM D2240
 4545Silicone Property, Side 1; ASTM D2240
Tensile Strength 5.34 MPa775 psiSilicone Property, Side 2; ASTM D412
 6.21 MPa900 psiSilicone Property, Side 1; ASTM D412
Elongation at Break 325 %325 %Silicone Property, Side 1; ASTM D412
 425 %425 %Silicone Property, Side 2; ASTM D412
Peel Strength 2.19 kN/m12.5 pliBond Strength; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 177 °C
0.250 hour
@Temperature 350 °F
Recommended Cure Cycle
 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month
@Temperature 21.1 °C
6.00 Month
@Temperature 70.0 °F
From date of manufacture
 
Descriptive Properties
ColorGray
Total Product Weight (oz/yd2)20.6Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay DAPCO™ 3041FR Paste Adhesive
Parker Chomerics Tecknit Teckfip™ FIP-E Formed in Place Conductive Elastomer
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray
Hexcel® Redux® 312L Modified epoxy film adhesive
Henkel Hysol EA 9360 Paste Adhesive System

PARL632 / 125818

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.