MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Synthos SUNCOATâ„¢ CR-20 Chlorinated rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SUNCOATâ„¢ chlorinated rubber is a derived product modified from the natural rubber through chlorination. It finds wide application in the production of coatings, inks, adhesives, etc. The company has a working capacity of 3500 tons of the chlorinated rubber with advanced technology and fine equipment. The quality of the product is stable and reliable. The product is trustworthy and well received by the customers. In coatings to remarkably improve the coating properties such as weatherability and water resistance, insulation, inflammability, anti-acidity, anti-alkali, adhesion as well as impact strength The chlorinated rubber coatings is widely applied to surface protection of materials for severe situation, such as shipping, offshore platforms, bridges, docks, containers, motor vehicle chassis, road signs, chemical equipment, etc. Additionally, high viscosity chlorinated rubber is applied to high-strength adhesives production, or added into other rubber products to improve its quality, while the low-viscosity product is applied to high-grade ink making.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 16 - 24 cP16 - 24 cP20% in xylene
Ash <= 0.30 %<= 0.30 %
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl >= 64 %>= 64 %
 
Descriptive Properties
AppearanceWhite or pale-yellow loose and soft powders
Heat stabilityStable under 130?

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW090 / 320121

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.