MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Matexcel NAT-183 Sodium Hyaluronate, cosmetic grade, >1800 kDa
Categories: Wood and Natural Products

Material Notes: This product is high molecular weight sodium hyaluronate and can be used in skin care products, beauty products, cleansing products, and hair products.

Application: HA is the best natural moisturizing component used in cosmetics .It has a good Compatibility and can be added in various cosmetics such as cream ,lotion .Cosmetic water ,essence, facial cleanser, liquid for bath ,shampoo and protect hair lotions ,mousse, lip stick.

Morphology: White powder

Key Words: Synonyms: HA, Hyaluronan, Hyaluronate, Sodium hyaluronate, Poly(b-glucuronic acid-[1?3]-b-N-acetylglucosamine-[1?4]); a-?UA-(1?42)-GlcNAc; sodium hyaluronate powder, hyaluronic acid; hyalobarrier gel; haluronic acid; hyaluronic acid sodium; hyaluronic acid na-salt;
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight >= 1.80e+6 g/mol>= 1.80e+6 g/mol
Storage Temperature 2.00 - 8.00 °C35.6 - 46.4 °F
 
Descriptive Properties
CAS Number9067-32-7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1213 / 299844

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.