MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 540 Polyurethane Sealant
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They bond to a wide variety of materials including plastics, metals, fiberglass, and wood. They are formulated to have a wide variety of Shore A hardness, open times, and performance parameters to meet many application needs.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³
Volatile Organic Compounds (VOC) Content 53.7 g/l53.7 g/l
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM C661
Tensile Strength at Break 2.10 MPa305 psiASTM D412
Elongation at Break >= 600 %>= 600 %ASTM D412
100% Modulus 0.900 MPa
@Strain 100 %
131 psi
@Strain 100 %
ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourRate of Cure, 50% RH
Tack-Free Time 60.0 - 90.0 min1.00 - 1.50 hour50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mearthane Durethane™ S DS-340A Solid Polyurethane Elastomer
Mearthane Durethane™ S DS-240A Solid Polyurethane Elastomer
Mearthane Durethane™ C 30-55A Polyurethane
Dow BETAMATE™ 7200 Polyurethane Prepolymer
Covestro DESMODUR® TD6400 + BAYTEC® XL TMP-TIPA + PLASTICIZER V10 (Catalyst SD6-40), 40 A Polyurethane, TDI- Ester

PMM33159 / 167906

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.