MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description

Polyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance and high heat resistance. These grades are available in improved scratch/mar resistant versions.
Application

These grades are suitable for automotive interior applications.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Melt Index of Compound 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.0 MPa50 mm/min, type I bar; ASTM D638
Elongation at Break >= 600 %50 mm/min, type I bar; ASTM D638
Elongation at Yield 10 %50 mm/min, type I bar; ASTM D638
Flexural Modulus 0.690 GPa70°C, 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790
 2.10 GPa1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790
 4.30 GPa
@Temperature -30.0 °C
1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790
Izod Impact, Notched 320 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASHU178 / 25142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.