Hostacom HYG 343L 356015 is a glass fiber reinforced PP homopolymer with very high melt flow rate. Product is UL listed. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: White Goods Market: Electrical / Electronics Processing Method: Injection Molding Information provided by LyondellBasell. |