MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm WEARTEC SF Cold Work Tool Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Cold Work Steel

Material Notes: Chromium-molybdenum-vanadium alloyed steel

The WEARTEC SF steel grade is a very highly alloyed spray formed cold work tool steel with a combination of extremely high wear resistance and a good resistance to cracking. WEARTEC SF is suitable for rolls and rotary knives with very high demands on abrasive wear resistance and carbide applications requiring toughness.

WEARTEC SF is characterized by:

  • Excellent abrasive wear resistance
  • High compressive strength
  • Good toughness
  • Good dimensional stability at heat treatment and in service
  • Very good through hardening properties
  • Very good resistance to tempering back
  • Good WEDM properties
  • Good surface treatment properties

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.264 lb/in³hardened to 62 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 270Soft annealed (Delivery condition)
Hardness, Rockwell C 43 - 67temper temp 210-1290°F (2 x 2h)
Modulus of Elasticity 30800 ksi(hardened to 62 HRC)
 27700 ksi
@Temperature 399 °C
hardened to 62 HRC
 28800 ksi
@Temperature 199 °C
hardened to 62 HRC
Compressive Yield Strength 1550 MPa0.2%, hardened to 50 HRC
 2450 MPa0.2%, hardened to 60 HRC
 2800 MPa0.2%, hardened to 64 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F
@Temperature 199 °C
hardened to 62 HRC
 6.40 µin/in-°F
@Temperature 399 °C
hardened to 62 HRC
Specific Heat Capacity 0.110 BTU/lb-°Fhardened to 62 HRC
Thermal Conductivity 17.0 W/m-K
@Temperature 199 °C
hardened to 62 HRC
 20.0 W/m-K
@Temperature 399 °C
hardened to 62 HRC
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.8 %
Chromium, Cr 7.0 %
Iron, Fe 77.5 %As Balance
Manganese, Mn 0.70 %
Molybdenum, Mo 2.3 %
Silicon, Si 0.80 %
Vanadium, V 8.9 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Crucible Steel CPM® 15V® Tool Steel
ATI Allegheny Ludlum A7 Tool Steel, UNS T30107
Crucible Steel CPM® 10V® (AISI A11) Tool Steel
Assab Steels ASP 23 Cold Work Steel
Bohler-Uddeholm ROLTEC SF Cold Work Tool Steel

NBUCOR38 / 15507

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.