MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dow™ DMDA-8950 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDA-8950 NT 7 HDPE is produced via UNIPOL™ Process Technology from Dow and is intended for use in thin-wall injection molding applications such as food containers, including freezer applications. This resin has been designed to provide a good impact/stiffness balance as well as excellent processability.
Main Characteristics:
  • Injection molding
  • For injection molded thin-wall food containers, including freezer applications
  • High flow for processing ease
  • Very narrow molecular weight distribution
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D792
ESCR 100% Igepal® 6.0 hour
@Temperature 50.0 °C
6.0 hour
@Temperature 122 °F
F50; ASTM D1693
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 21.3 MPa3090 psiASTM D638
Tensile Strength, Yield 20.9 MPa3030 psiASTM D638
Elongation at Break 37 %37 %ASTM D638
Elongation at Yield 9.0 %9.0 %ASTM D638
Flexural Modulus 0.576 GPa83.5 ksi2% Secant; ASTM D790B
Tensile Impact Strength 90.3 kJ/m²43.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 127 °C260 °F
Crystallization Temperature 115 °C239 °F
Brittleness Temperature -52.8 °C-63.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF454 / 311147

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.