MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Desmodur® Z 4470 MPA/X Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Aliphatic polyisocyanate (IPDI trimer). As the hardener component for lightfast polyurethane coating systems and as an additive resin for alkyd spray coatings.

Properties / Applications: Desmodur® Z 4470 MPA/X is used primarily as the hardener component for lightfast two-component polyurethane coatings with high resistance to chemicals and weathering, very good gloss retention and outstanding mechanical properties. On account of its high hardness, Desmodur® Z 4470 MPA/X is normally mixed with Desmodur® N products. Preferred co-reactants are flexibilised polyacrylate polyols such as Desmophen® A 565 and A 575 and polyester polyols such as Desmophen® 670. The main applications for two-component coatings based on Desmodur® Z 4470 MPA/X are in automotive OEM and automotive refinishing. As Desmodur® Z 4470 MPA/X has very good physical drying properties, it is also used as an additive resin in alkyd spray coatings to accelerate drying. The main applications of such coatings are in automotive refinishing and industrial finishing.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccDIN EN ISO 2811
Volatiles 28 - 32 %28 - 32 %0.2 g/1 h/120 °C; M020-ISO 3251
Viscosity 1000 - 2000 cP1000 - 2000 cPM014-ISO 3219/A.3
 
Thermal PropertiesMetricEnglishComments
Flash Point 40.0 °C104 °FDIN 53 213/1
 
Descriptive Properties
Color<60Hazen, M017-EN 1557
Content<0.35%Monomeric IPDI, M106-ISO 10283
 11.5-12.3%NCO, M105-ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0676 / 202459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.