MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Parson Adhesives PARFIX® 3382 High Viscosity Cyanoacrylate Adhesives
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3382 is a high viscosity combined with fast cure speed, one component adhesive especially recommended for electronic applications. This product is formulated for use with PARFIX activators for tacking electronic components.

Applications:

  • Ideal for bonding Rubbers, Metals and Plastics.
  • Ideal for tack jumper wires and wires to coil forms. Small appliances, electronic parts, Computer peripherals, etc.
  • Mounting standoffs, edge guides, and stiffeners to circuit boards.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.126 g/cc0.00455 lb/in³
Brookfield Viscosity 5000 cP5000 cPRVT
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 6.00 MPa870 psiPVC; ASTM D1002
 7.03 MPa1020 psiPolycarbonate; ASTM D1002
 7.03 MPa1020 psiABS; ASTM D1002
 10.0 MPa1450 psiSBR Rubber; ASTM D1002
 12.0 MPa1740 psiNeoprene Rubber; ASTM D1002
 12.0 MPa1740 psiNitrile Rubber; ASTM D1002
 19.0 MPa2760 psiAluminum; ASTM D1002
 13.0 - 28.0 MPa1890 - 4060 psi
 28.0 MPa4060 psiSteel; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 24.6 kV/mm625 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Glass Transition Temp, Tg 122 °C252 °FASTM E228
 135 °C275 °FCured; ASTM E228
Flash Point >= 87.0 °C>= 189 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
 
Descriptive Properties
AppearanceClear liquid
CompositionEthyl Cyanoacrylate
Gap Filling0.7 mm
Initial Strength Retained (%)7500Gasoline for 1000 hrs at 22°C
 8000Gasoline for 500 hrs at 22°C
 8500Isopropanol for 500 hrs at 22°C
 8500Isopropanol for 1000 hrs at 22°C
 9000Motor Oil for 500 hrs at 40°C
 9000Motor Oil for 1000 hrs at 40°C
 9000Mineral Spirit for 500 hrs at 22°C
 9000Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN113 / 186556

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.