MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV X11059DB Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 11000 series are engineered low friction slip coating materials designed primarily for demanding automotive and industrial applications. This product is a high hardness, low density grade with good UV resistance and superior abrasion resistance are co-extruded with TPE-S, TPE-V and EPDM.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Abrasion Resistant; Bondability; Chemical Resistant; Good Adhesion; Good Processability; High Hardness; High Heat Resistance; High Tensile Strength; Low Compression Set; Low Density; Low Friction; Low Specific Gravity; Specialty Grade; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Coating Applications; Industrial Applications; Rubber Replacement; Weatherstripping

RoHS Compliance: RoHS Compliant

Automotive Specifications: DAIMLER DBL 5578 Color: Black; VAG VW501 23 Color: Black

Form: Pellets

Processing Method: Coextrusion; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Viscosity 552 cP
@Shear Rate 206 1/s,
Temperature 200 °C
552 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60
@Time 5.00 sec
60
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 24.0 MPa3480 psiAcross Flow; ISO 37
 28.0 MPa4060 psiFlow; ISO 37
Elongation at Break 30 %30 %Flow; ISO 37
 99 %99 %Across Flow; ISO 37
Tear Strength 94.7 kN/m540 pliMethod Ba, Angle (Unnicked); ISO 34-1
 
Processing PropertiesMetricEnglishComments
Zone 1 177 - 210 °C350 - 410 °F
Zone 2 182 - 216 °C360 - 420 °F
Zone 3 193 - 227 °C380 - 440 °F
Zone 4 193 - 227 °C380 - 440 °F
Zone 5 193 - 227 °C380 - 440 °F
Die Temperature 193 - 227 °C380 - 440 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stellarchem SV-B65E TPV Compound
Avient Elastamax™ XL 0162-28 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-25 EPDM TPV-Based Thermoplastic Elastomer
Teknor Apex Sarlink® TPV 3470N Thermoplastic Vulcanizate
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer

PTEKNQ1228 / 237719

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.