MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plastcom SLOVAMID 6 GF 10 Polyamide 6, 10% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Features

PA 6 for injection moulding, chemically strengthened with 10% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and consumer-goods industry, eg.: grips for electro tools, hobby tools, gears, cases of the electrotools, cooling screws of blowers, electromotors, carrying parts in the automotive industry. With the increasing content of GF also the toughness, flexural and tensile strength increase as well as the heat application increases up to 150°C and the shrinkage decreases. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0074 cm/cm0.0074 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0165 cm/cm0.0165 in/inSTN 64 0808
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psiSTN EN ISO 527-2
Elongation at Break 4.0 %4.0 %STN EN ISO 527-2
Tensile Modulus 4.90 GPa711 ksiSTN EN ISO 527-2
Flexural Strength 145 MPa21000 psiSTN EN ISO 178
Flexural Modulus 3.90 GPa566 ksiSTN EN ISO 178
Charpy Impact Unnotched  1.70 J/cm²
@Temperature -20.0 °C
8.09 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 0.270 J/cm²
@Temperature 23.0 °C
1.28 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FSTN EN ISO 75/A
Vicat Softening Point 195 °C383 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °FSTN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Plastcom SLOVAMID 6 GF 15 HI PA6, 15% glass fibre, improved strength
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre
Global Atron 602 GF-13 Natural Nylon 6, 13% Glass Filled
Envalior Akulon® K223-HGM24 PA6-(GF+MD)30, Dry, 10/20% Glass/Mineral Filled, Heat Stabilized

PPLACO006 / 106884

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.