Property data reported is normalized to 60% fiber volume. Cured with #2500 epoxy at 130 °C. Baseline carbon fiber with a 40-year production history and is known for its balanced composite properties, high quality, consistency, reliability and suppliability. Excellent processability in traditional manufacturing methods (weaving, braiding, filament winding, prepreg, etc.). Information provided by Toray Composite Materials America, Inc. |