MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 15370T020 0.020" (0.508 mm) Uncatalyzed, Unsupported Rubber on a Mylar Carrier
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Design/Construction:
Side 1: Uncatalyzed, Unsupported Rubber on a Mylar Carrier

Appearance: Translucent high viscosity gum

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.50 milMylar Carrier
 3.00 milPoly Interleave
 18.0 - 22.0 milOverall
 18.0 - 22.0 milSide 1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 23.9 °C
From date of manufacture
 
Descriptive Properties
ColorBlueInterleave
 Naturally Translucent
Total Product Weight (oz/yd2)19Compound Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave
Rogers Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Rogers Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge
DuPont Teijin Films Mylar® 823 Polyester Film, 48 Gauge

PARL113 / 125299

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.