MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion
Categories: Polymer; Thermoset; Polyurethane, TS; Silicone

Material Notes: 1KSP is a silicone modified polyurea dispersion “Powered by ReactAmine® Technology” designed for a wide range of rigid and flexible substrates such as wood, metal, vinyl, concrete and other plastic parts. 1KSP is an excellent primer for concrete, metal, PVC and wood prior to applying polyureas. A key application is coating concrete, polyurethane, and polyurea bed liners to improve weatherability and color retention. This product has been developed to exhibit a combination of film hardness, flexibility, good water and abrasion resistance, and excellent solvent resistance. This product can be ordered with antimicrobial additives. The 1KSP has anti-graffiti characteristics. 1KSP May be cross linked with a special water dispersible aliphatic isocyanate to improve chemical resistance and toughness. Levels of 5-10% based on solids, should be added. On porous concrete, it is recommended to first apply primer 1K59. This will fill up the pores in the concrete, yielding excellent adhesion to concrete. After the 1KP59 is dry to touch, apply 1KPSP clear or colored.

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.90 lb/ft³
Solids Content 37 %by Volume
pH 7.5 - 9.5
Viscosity 5.0 - 30 cP@ 275
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 30T 2.0 - 3.0Pencil, 1KSP+5%A
Tensile Strength 5980 psi
 6520 psi1KSP+5%A
Elongation at Break 150 %1KSP+5%A
 210 %
Abrasion 1.6mg loss
 
Descriptive Properties
ColorClearFilm
 Milky, White
Freeze Thaw StabilityPassed 5 cycles
Hot TireNo Stain
Plasticizer (1 hour)50 (Failure)-5 (Excellent)
Resistance to Acetone (10 seconds)Excellent
Resistance to Alcohol (1 hour)Failure
Resistance to Alcohol/Water 1:1 (1 hour)10 (Failure)-5 (Excellent)
Resistance to Ammonia (1 hour)4-50 (Failure)-5 (Excellent)
Resistance to Brake Fluid (2 hours)No effect
Resistance to Brake Fluid (24 hours)Failure
Resistance to Coffee (16 hours)40 (Failure)-5 (Excellent)
Resistance to Diesel Fuel (24 hours)No effect
Resistance to GasolineNo effect
Resistance to Motor Oil (24 hours)No effect
Resistance to Nivea (16 hours)Excellent
Resistance to Pepsi Cola (24 hours)No effect
Resistance to Transmission Fluid (24 hours)No effect
Resistance to Water (16 hours)Excellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron L060330-2 Flexible Polyurea Compound
CHT Group EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea
CHT Group EP 2KSP EPI Engineered Polymers Silicone Modified Polyurea
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade

PACC096 / 22223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.