MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate (PC)

Material Notes: EMERGE™ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. Its superior processing makes it ideal for molding large parts and optimizing cycle time productivity in injection molding operations. It has a UL 94 flammability rating of V-0 at 1.5mm. This resin is suitable for use in a wide variety of applications in the information technology equipment and consumer electronic markets. Applications included: TV enclosures, monitor enclosures, PC enclosures, adaptors and chargers.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
Melt Flow 20 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 75 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039/2
Tensile Strength at Break 46.2 MPa3.2 mm, Injection Molded; ASTM D638
Tensile Strength, Yield 62.1 MPa3.2 mm, Injection Molded; ASTM D638
Elongation at Break 50 %3.2 mm, Injection Molded; ASTM D638
Elongation at Yield 4.0 %3.2 mm, Injection Molded; ASTM D638
Flexural Strength 97.9 MPa3.2 mm, Injection Molded; ISO 178
Flexural Modulus 2.80 GPa3.2 mm, Injection Molded; ISO 178
Izod Impact, Notched 370 J/m
@Thickness 3.20 mm
Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °Cunannealed; ASTM D256
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °Cunannealed; ASTM D256
Vicat Softening Point 108 °C120°C / 10N; ASTM D1525
Flammability, UL94 V-0
@Thickness 1.50 mm
all colors
Oxygen Index 29 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 250 °C
Mold Temperature 60.0 - 91.0 °C
Drying Temperature 79.0 - 91.0 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical AF342F ABS, Flame Retardant, High Flow
A. Schulman Diamond ASA/PC FA-30
A. Schulman Diamond ASA TW-15H
A. Schulman Diamond ASA T-110
A. Schulman Diamond ABS VP-11

PZZDOW1335 / 30553

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.