MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3HG7 BK 00564 35% Glass Filled PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced and heat aging resistant injection molding grade, e.g. for parts and components with high stiffness and dimensional stability as well as electrically insulating parts.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.4 - 1.8 %1.4 - 1.8 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.7 - 5.3 %4.7 - 5.3 %ISO 62
Viscosity Measurement 145145ISO 307
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inrestricted
Melt Flow 56.4 g/10 min
@Load 5.00 kg,
Temperature 275 °C
56.4 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 150 MPa21800 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 8.50 GPa1230 ksiISO 527-1/-2
Flexural Strength 240 MPa34800 psiat max force; ISO 178
Flexural Modulus 8.50 GPa1230 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 6600 MPa
@Strain <=0.5 %
957000 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.7
@Frequency 1e+6 Hz
5.7
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.15
@Frequency 1e+6 Hz
0.15
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 140 °C284 °Ffor 50% loss of tensile strength after 20000hr
 170 °C338 °Ffor 50% loss of tensile strength after 5000hr
 240 °C464 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection-molding
 
Descriptive Properties
ColorBK 00564
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3HG7 BK 00564 35% Glass Filled PA66 (Dry)
BASF Ultramid® Structure B3WG10 LF High-Performance Long-Glass Fiber Reinforced Polyamide
BASF Ultramid® A3X4G7 BK 23079 35% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Dry)
BASF Ultramid® A3WG7 HP BK 20560 35% Glass Filled PA66 (Conditioned)

PBASG0240 / 131873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.