BASF Ultramid® B3K BK00464 PA6 (Dry)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Unreinforced
Material Notes:
Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.13
g/cc
0.0408
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
2.6 - 3.4 %
2.6 - 3.4 %
23°C; 50% RH; ISO 62
Water Absorption at Saturation
9.0 - 10 %
9.0 - 10 %
ISO 62
Viscosity Measurement
150
150
ISO 307
Linear Mold Shrinkage
0.0065
cm/cm
0.0065
in/in
restricted
Melt Flow
180.8
g/10 min
@Load 5.00 kg,
Temperature 275 °C
180.8
g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
85.0
MPa
12300
psi
50 mm/min; ISO 527-1/-2
Elongation at Yield
4.5 %
4.5 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity
3.00
GPa
435
ksi
ISO 527-1/-2
Flexural Modulus
2.80
GPa
406
ksi
ISO 178
Izod Impact, Notched (ISO)
5.00
kJ/m²
@Temperature -30.0 °C
2.38
ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
5.50
kJ/m²
@Temperature 23.0 °C
2.62
ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched
10.0
J/cm²
@Temperature -30.0 °C
47.6
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.400
J/cm²
@Temperature -30.0 °C
1.90
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
0.550
J/cm²
@Temperature 23.0 °C
2.62
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+13
ohm-cm
1.00e+13
ohm-cm
IEC 60093
Dielectric Constant
3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor
0.032
@Frequency 1e+6 Hz
0.032
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
600
V
Test solution A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
70.0
-
100
µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9
-
55.6
µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Specific Heat Capacity
1.70
J/g-°C
0.406
BTU/lb-°F
Thermal Conductivity
0.330
W/m-K
2.29
BTU-in/hr-ft²-°F
DIN 52612
Melting Point
220
°C
428
°F
DIN 53765
Maximum Service Temperature, Air
100
°C
212
°F
for 50% loss of tensile strength after 20000hr
112
°C
234
°F
for 50% loss of tensile strength after 5000hr
180
°C
356
°F
Deflection Temperature at 0.46 MPa (66 psi)
180
°C
356
°F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
65.0
°C
149
°F
ISO 75-1/-2
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Processing Properties
Metric
English
Comments
Melt Temperature
250
-
270
°C
482
-
518
°F
Injection-molding/Extrusion
Mold Temperature
40.0
-
80.0
°C
104
-
176
°F
Injection-molding
Descriptive Properties
Commercial Status
Europe
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultramid® B3K BK00464 PA6 (Conditioned)
BASF Ultramid® B3L BK00464 PA6 (Dry)
BASF Ultramid® 8253 PA6 (Conditioned)
BASF Ultramid® B3K PA6 (Dry)
BASF Ultramid® B3S BK00464 PA6 (Dry)
PBASG0250 / 131883
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.