MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Braskem TS9003 LDPE Blown Film Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packaging with a good appearance, a low level of breakage, and an elevated support structure during manual transport. It also presents flow properties that ensure an excellent processability in conventional extruders for LDPE, granting low energy consumption during the whole process and allowing for the production of films with good dimensional uniformity and excellent surface finishing. The incorporated additives package warrants thermal stability during processing and a low coefficient of friction (COF), which are indispensable for high productivity on the printing, cutting and welding, and shrink-wrap lines. This product is identified as PE 125 according to ASTM D-4976-04a standard specification. TS9003 contains antiblocking agent and slip agent additives. Its applications include: technical shrink-wrap films for unitization of various products (soft drink and mineral water bottles, soft drink cans, beers, paints, etc.) and monolayer and multi-layer technical films (coextrusion or laminated) for packages that need gloss associated with mechanical resistance and greater stiffness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³ASTM-D792
Melt Flow 0.27 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 370 %370 %ASTM-D882
Film Elongation at Break, TD 700 %700 %ASTM-D882
Secant Modulus, MD 0.170 GPa24.7 ksi2% Secant Modulus; ASTM-D882
Secant Modulus, TD 0.180 GPa26.1 ksi2% Secant Modulus; ASTM-D882
Elmendorf Tear Strength MD 210 g210 gASTM-D1922
Elmendorf Tear Strength TD 260 g260 gASTM-D1922
Elmendorf Tear Strength, MD 4.20 g/micron107 g/milASTM-D1922
Elmendorf Tear Strength, TD 5.20 g/micron132 g/milASTM-D1922
Dart Drop 2.40 g/micron61.0 g/milASTM-D1709
Dart Drop Test 120 g0.265 lbASTM-D1709
Film Tensile Strength at Break, MD 25.0 MPa3630 psiASTM-D882
Film Tensile Strength at Break, TD 24.0 MPa3480 psiASTM-D882
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM-D1003
Gloss 53 %53 %Angle 45°; ASTM-D2457
 79 %79 %Angle 60°; ASTM-D2457
 
Processing PropertiesMetricEnglishComments
Die Opening 0.100 cm0.0394 inBlow Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0Blow Film Extrusion
 
Descriptive Properties
Mass Temperature (°C)180-220Blow Film Extrusion
Temperature Profile (°C)150-195Blow Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation
PolyMirae Moplen HP526N IPP/WQBF Grade Polypropylene
Petroquimica Triunfo Trithene® TS 8090 MDPE - Thermal Shrink Film
Petroquimica Triunfo Trithene® TE 8088 MDPE - Thermal Shrink Film
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend

PBRAS834 / 106680

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.