MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller HP008 Hot Melt Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: HP008 is single component hot melt adhesive that cross-links through a chemical reaction with moisture found in the atmosphere and substrates to form a set adhesive. HP008 is a high performance, high green strength grade reactive hot melt with superior adhesion to a variety of substrates. It can be applied using roll coaters, as well as hot melt adhesive guns. It is particularly suited for bonding EPS, PU foam, aluminum, steel, various plastics (PVC, ABS, and SMC), and rubber.

Features and Benefits:

  • High green strength
  • Good heat resistance
  • High adhesion on a variety of substrates
  • High toughness
  • 100% solid

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 8000 - 11000 cP
@Temperature 121 °C
8000 - 11000 cP
@Temperature 250 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.345 MPa>= 50.0 psiGreen
 17.2 MPa2490 psi
Elongation at Break 250 %250 %
2% Secant Modulus 0.0138 GPa2.00 ksi
 
Processing PropertiesMetricEnglishComments
Cure Time 0.750 - 1.00 min0.0125 - 0.0167 hourRoll Coater Open Time
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
ColorOff White
ConsistencyViscous LiquidSolid at Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL167 / 316958

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.