MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC NORYL™ FE1410PW PPE+PS (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: NORYL™ FE1410PW resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + crystal clear polystyrene (ccPS). This injection moldable material is FC EU, FDA food contact compliant, NSF/ANSI 61*, ACS, WRAS, KTW, and W270 listed for global potable water use. NORYL FE1410PW resin exhibits excellent long-term hydrolytic stability, very low moisture absorption, heat / hot water resistance and is an excellent candidate for a variety of water management applications such as pump housings, impellers, shower/faucet, membrane housings and valves. *NSF certification is color dependent.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.060 %0.060 %50% RH; ASTM D570
Water Absorption at Saturation 0.20 %0.20 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 32 g/10 min
@Load 10.0 kg,
Temperature 280 °C
32 g/10 min
@Load 22.0 lb,
Temperature 536 °F
MVR [cc/10 min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 94.0 MPa13600 psi5 mm/min; ISO 527
 94.0 MPa13600 psi5 mm/min; ASTM D638
Elongation at Break 2.7 %2.7 %5 mm/min; ISO 527
 2.8 %2.8 %5 mm/min; ASTM D638
Tensile Modulus 4.77 GPa692 ksi5 mm/min; ASTM D638
 4.93 GPa715 ksi1 mm/min; ISO 527
Flexural Strength 135 MPa19600 psibreak, 2 mm/min; ISO 178
 135 MPa19600 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.86 GPa705 ksi1.3 mm/min, 50 mm span; ASTM D790
 4.88 GPa708 ksi2 mm/min; ISO 178
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM D256
 0.350 J/cm
@Temperature -30.0 °C
0.656 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 2.30 J/cm4.31 ft-lb/inASTM D4812
 2.25 J/cm
@Temperature -30.0 °C
4.22 ft-lb/in
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1U
 13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 1.40 J/cm²6.66 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/2C
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
16.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 126 °C259 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 127 °C
@Thickness 3.20 mm
261 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 140 °C284 °FRate B/120; ISO 306
 146 °C295 °FRate A/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 280 - 300 °C536 - 572 °FInjection Molding
Zone 1 250 - 270 °C482 - 518 °F
Zone 2 270 - 290 °C518 - 554 °FInjection Molding
Zone 3 290 - 310 °C554 - 590 °F
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %Injection Molding

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH90244 / 251368

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.