MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Vulkasil® N Precipitated Silica Filler for Rubber
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: The properties of technical rubber compounds and their vulcanizates depend not only on the polymer but also to a significant degree on the other ingredients and their proportions. Among these ingredients, fillers are very important. Without reinforcing fillers (white fillers or carbon black), the manufacture of serviceable vulcanizates from polymers that are not self reinforcing, such as natural rubber and many synthetic rubbers, is impossible. Vulkasil® is produced from aqueous sodium silicate solution by precipitation with acids or metal salt solutions (aluminium sulfate). The mechanical properties of rubber compounds, such as hardness, modulus, strength, tear propagation resistance and abrasion resistance, are improved, and the use of different colors is possible. Vulkasil® fillers are used together with other white fillers, such as china clay and talc, for various vulcanizates needing particularly good resistance to aging. The resistance of the resulting vulcanizates to hot air aging is often superior to that of goods produced with carbon black. Precipitated silica plays an important part in the bonding of rubber to fabric or to steel cord.

Key Properties

  • Fillers with medium to strong reinforcing effect
  • improved resistance to hot air aging and abrasion
  • improved bonding of rubber to fabric or to steel cord

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/cc
Volatiles 4.0 - 7.0 %
@Temperature 105 °C,
Time 7200 sec
DIN ISO 787/2
pH 6.3 - 7.55% in water; DIN ISO 787/9
Specific Surface Area 110 - 150 m²/gISO 9277
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1000 ohm-cm4% in water, DIN ISO 787/14
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearancewhite amorphous powder
Specifications<0.1%Sieve residue (0.063 mm), DIN ISO 787/18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Vulkasil® S/KG Precipitated Silica Filler for Rubber
Lanxess Vulkasil® S Precipitated Silica Filler for Rubber
Lanxess Vulkasil® C Precipitated Silica Filler for Rubber
Lanxess Vulkasil® A1 Precipitated Silica Filler for Rubber
Silicon Dioxide, SiO2 (Alpha Cristobalite)

PLANY9177 / 209568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.